Influencing Factors and Control Strategies for Blistering in Neutral Wall Putty: An Experimental Analysis Based on HPMC Dosage, Viscosity, and Ground Calcium Carbonate Fineness

During the application of neutral wall putty, blistering may appear on the surface as bulges in the putty layer, pinholes, small pits, or localized ruptured bubbles. In essence, these defects indicate that air within the slurry system has not been released smoothly. The air may be introduced ...